Reduction of TiO2 content in a sample of Iron ore from Khursipar area (Maharashtra)

Ranganathan, M V and Subramanya, G V and Narayanan, P I A (1962) Reduction of TiO2 content in a sample of Iron ore from Khursipar area (Maharashtra). Other (TMP). CSIR-NML, Jamshedpur, Jamshedpur.

[thumbnail of Reduction of TiO2 content in a sample of Iron ore from Khursipar area (Maharashtra)] PDF (Reduction of TiO2 content in a sample of Iron ore from Khursipar area (Maharashtra))
I.R_233-62.pdf - Published Version
Restricted to NML users only. Others may use ->

Download (3MB) | Request a copy

Abstract

A Sample of titaniferous iron ore received from the Director of Geology and Mining, Government of Maharashtra, assayed 55.7% Fe, 15.11% TiO2, 6.5% FeO, 2.1% SiO2, 1.05% Al2O3, 0.70% MgO, 0.009% P and 0.005% S. continuous wet magnetic separation of the sample crushed to -10 mesh size followed by grinding of the magnetic concentrate obtained, to -65 mesh and magnetic separation yielded a final magnetic concentrate assaying 63.05% Fe, and 9.9% TiO2 with a recovery of 71.1% Fe. It is suggested that the magnetic concentrate, may be smelted after suitable agglomeration.

Item Type: Project Reports (Other (TMP))
Uncontrolled Keywords: Khursipar area-Maharashtra, iron-ore, reduction of TiO2,magnetic separation, agglomeration, titaniferous iron ore
Subjects: Chemical Engineering
Divisions: Information Management and Dissemination Centre
Depositing User: Users 43 not found.
Date Deposited: 01 Apr 2022 12:01
Last Modified: 13 Jun 2022 09:12
URI: http://eprints.nmlindia.org/id/eprint/8560

Actions (login required)

View Item
View Item