Abhilash, and Pandey, B D (2013) Microbial processing of apatite rich low grade Indian uranium ore in bioreactor. Bioresource Technology, 128 (IF-4.980). pp. 619-623.
BITE10809.pdf - Published Version
Restricted to Repository staff only
Download (672kB) | Request a copy
Abstract
Bioreactor leaching using enriched culture of Acidithiobacillus ferrooxidans and Leptosprillium ferrooxidans was investigated for the apatite rich Indian (Narwapahar) uranium ore. Bioreactor leaching of Narwapahar ore of <45 lm size at pH 2.0 and 10% (w/v) PD using 10% (v/v) inoculum of the bacterium at 35oC (A.ferrooxidans) and 40 C (L. ferrooxidans), solubilised 57% and 63% uranium in 5 days, respectively; the E SCE
values being 561 and 588 mV. Leaching kinetics improved so much so that 83% uranium was recovered in just 10 h with 10% inoculum of A. ferrooxidans containing biogenic Fe3+; at 20% PD uranium recovery rose to 87%. Role of temperature (25–40 C) was noticed with 90.3% uranium bioleaching in 10 h at 40oC with L. ferrooxidans as against 77% leaching with A. ferrooxidans at pH 2.0, 40 C and 20% (w/v) PD.
| Item Type: | Article |
|---|---|
| Uncontrolled Keywords: | Uranium ores; Low-grade; Apatite; Mine microbes; Bioreactor |
| Subjects: | Metallurgy > Extractive Metallurgy > Hydrometallurgy Minerals and Mining Waste Management |
| Divisions: | Metal Extraction and Forming |
| Depositing User: | Dr. Abhilash . |
| Date Deposited: | 28 Jan 2013 05:20 |
| Last Modified: | 27 Dec 2013 12:25 |
| URI: | http://eprints.nmlindia.org/id/eprint/6337 |