Solvothermal synthesis of high value copper powder from copper bleed solution of an Indian copper smelter

Meshram, Pratima and Sinha, Manish K and Sahu, S K and Khan, Pritam and Pandey, B D and Mankhand, T R (2013) Solvothermal synthesis of high value copper powder from copper bleed solution of an Indian copper smelter. Powder Technology, 233 (IF-2.265). pp. 335-340.

[thumbnail of Powder_Technology.pdf] PDF
Powder_Technology.pdf - Published Version
Restricted to NML users only. Others may use ->

Download (1MB) | Request a copy

Abstract

Recovery of copper powder from copper bleed solution (CBS) of a copper smelter by solvothermal route has been investigated. After removing sulphuric acid by solvent extraction with tri-iso-octyl-amine, copper from the acid depleted CBS was recovered by using Versatic 10 acid as an extractant in kerosene. In 1.5 M Versatic 10 acid 29.8 g/L copper was loaded at an equilibrium pH of 4.25. During the hydrogen stripping, a 97% copper powder was recovered from the loaded Versatic 10 acid solution at 20 bar hydrogen pressure and 403 K temperature. The solvothermal synthesis of copper powder followed nucleation and growth kinetic
model with activation energy value of 145 kJ/mol. Stripping of copper powder could also follow the chemical control kinetic model with lower value of activation energy (66 kJ/mol). The copper powder as characterized by SEM exhibited globular particles of 0.25–0.5 μm size and was found to be suitable for P/M applications.

Item Type: Article
Uncontrolled Keywords: Copper bleed solution,Solvent extraction,Versatic 10 acid, Autoclave Solvothermal synthesis
Subjects: Metallurgy > Extractive Metallurgy > Hydrometallurgy
Divisions: Metal Extraction and Forming
Depositing User: Dr. Pratima Meshram
Date Deposited: 23 Oct 2012 06:03
Last Modified: 27 Dec 2013 12:24
URI: http://eprints.nmlindia.org/id/eprint/6159

Actions (login required)

View Item
View Item