Ray, Ajoy K and Venkateswarlu, K and Chaudhury, S K and Das, S K and Ravi Kumar, B and Pathak, L C (2002) Fabrication of TiN reinforced aluminium metal matrix composites through a powder metallurgical route. Materials Science and Engineering A, 338 (1-2). pp. 160-165.
Ajoy_Kumar_Ray.pdf - Published Version
Restricted to NML users only. Others may use ->
Download (514kB) | Request a copy
Abstract
Fabrication of Al–TiN (10, 30 wt.%) composites by a powder metallurgical route has been investigated using pressureless sintering and hot pressing techniques. Results indicate that sintering followed by hot pressing is required for significant densification and improvement of mechanical properties. The presence of titanium nitride (TiN) particles at grain boundaries played a significant role in improving the densification, and results in improved mechanical properties. Dry sliding wear results showed improved wear resistance of the composite (Al–TiN) compared to the base material (Al) metal due to presence of TiN particles. The wear rates of the Al–TiN composites decrease by an order of magnitude after hot pressing.
| Item Type: | Article |
|---|---|
| Uncontrolled Keywords: | Al–TiN composites; Metal matrix composite; Sintering; Hot pressing; Wear resistance |
| Subjects: | Metallurgy |
| Divisions: | Material Science and Technology |
| Depositing User: | Users 6 not found. |
| Date Deposited: | 18 Nov 2009 05:24 |
| Last Modified: | 02 Sep 2026 06:06 |
| URI: | http://eprints.nmlindia.org/id/eprint/283 |