The addition of TiC (5-10 wt.%) and C (5 wt.%) was found to enhance the sinterability of SHS produced ZrB2 powder. The densification increased to 94% of the theoretical density with the addition of carbon and TiC. The oxygen impurities normally present on the surface of this diboride powder leads to exaggerated grain-growth during sintering and hinders densification. The addition of C and TiC reduced the surface oxide layer and resulted in improved densification. Less gain-growth was also observed during sintering. (C) 2005 Elsevier B.V. All rights reserved.
Item Type: | Article |
---|---|
Official URL/DOI: | DOI: 10.1016/j.matlet.2005.06.015 |
Uncontrolled Keywords: | ZrB2; ceramics; SHS; high temperature material and sintering |
Divisions: | Material Science and Technology |
ID Code: | 3333 |
Deposited By: | Sahu A K |
Deposited On: | 14 Jul 2011 17:18 |
Last Modified: | 25 Jan 2012 10:18 |
Related URLs: |
Repository Staff Only: item control page