Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar

Chintala, Rajesh and Rath, R K and Kumar, Anil (2017) Effective Utilization of Fly Ash, Iron Ore Slime and LD-Slag in Geopolymer Mortar. Recent Trends in Civil Engineering & Technology, 7(1). pp. 9-16.

[thumbnail of 7973-25409-1-PB_final.pdf] PDF
7973-25409-1-PB_final.pdf
Restricted to NML users only. Others may use ->

Download (661kB) | Request a copy
Official URL/DOI: http://www.nmlindia.org

Abstract

An attempt was made for the effective utilization of iron ore slime in making of geopolymer mortar along with other industrial wastes fly ash and LD-slag and achieved the appreciable compressive strength results with 8 M NaOH after 28 days at a curing period of 24 h at 55°C.

Item Type: Article
Uncontrolled Keywords: Fly ash, LD-slag, geopolymer, compressive strength, NaOH, iron ore slime
Subjects: Minerals and Mining
Divisions: Mineral Processing
Depositing User: Dr. R.K. Rath
Date Deposited: 28 Nov 2017 04:41
Last Modified: 03 Sep 2026 14:09
URI: http://eprints.nmlindia.org/id/eprint/7722

Actions (login required)

View Item
View Item