Internal hydrogen embrittlement of cold drawn steels

Singh, Inder and Banerjee, M K and Nag, P S (1981) Internal hydrogen embrittlement of cold drawn steels. Transactions of The Indian Institute of Metals, 34 (6). pp. 433-439.

[thumbnail of 433-439_1981.PDF] PDF
433-439_1981.PDF
Restricted to NML users only. Others may use ->

Download (2MB) | Request a copy

Abstract

Recent studies have indicated that hydrogen embritt-lement is a result of lowering of lattice cohesion and build up high internal pressure microcrack. The effect of prior plastic deformation on TTF (Total Time to fracture)of sustained tensile loaded steel under cathodic hydro-genation condition has been studied. The effect of incr-easing cathodic current, cold reduction, poison (As2O3) and the effect of dynamic tensile loading on TTF have also been studied.

Item Type: Article
Uncontrolled Keywords: Internal hydrogen; lattice decohesion; melting; pickling
Subjects: Materials Science
Divisions: Corrosion and Surface Engineering
Depositing User: Users 5 not found.
Date Deposited: 16 May 2012 06:27
Last Modified: 05 Feb 2013 09:03
URI: http://eprints.nmlindia.org/id/eprint/5184

Actions (login required)

View Item
View Item