Damage Assessment of Process Heater Tube by Magnetic Technique :A Case Study

Mitra, A (2001) Damage Assessment of Process Heater Tube by Magnetic Technique :A Case Study. In: UNSPECIFIED.

[thumbnail of 39-45.PDF] PDF
39-45.PDF
Restricted to NML users only. Others may use ->

Download (1MB)

Abstract

Ferromagnetic properties of steel change with the microstructure, composition and the stress state of the materials. Such variations are also taking place when
the steel components are in service. Hence magnetic techniques may be used as a potential tool for integrity assessment of engineering components. The present work deals with the magnetic characterisation of process heater tube made of austenitic steel HP-40 grade employed in naphtha cracking unit of a petrochemical industry. The tube was non-magnetic in the virgin state and became magnetic during service exposure. The origin of magnetism in service exposed tube will be discussed here. Feasibility of using magnetic nondestructive evaluation technique for damage assessment of the studied process
heater tube will also be explored in the present investigation.

Item Type: Conference or Workshop Item (UNSPECIFIED)
Uncontrolled Keywords: Magnetic Technique; Ferromagnetic Properties
Subjects: Materials Science
Divisions: Material Science and Technology
Depositing User: Users 5 not found.
Date Deposited: 19 Apr 2011 16:18
Last Modified: 13 Jan 2012 07:00
URI: http://eprints.nmlindia.org/id/eprint/2765

Actions (login required)

View Item
View Item